    Two factor authentication (for most of you 'email a code') has been temporarily disabled while we figure out why emails are not being received by large numbers of users. Emails are not sending site-wide. Please continue to use AF-UK as normal but note that you may be asked to log back in once this is re-enabled.

Stripping anodisation from aluminium

Seven

Members
Joined
Jun 7, 2018
Messages
391
Reaction score
77
Well smack my ass and call me daddy, caustic soda is da shit!

Supplier was out of stock of the silver slide I wanted so ordered the black one with the intention of stripping the anodisation back to the original silver aluminium.

Little bit of research, little bit of prep and safety and viola!

One very clean slide!

Now the polishing to a mirror finish begins...

View attachment 42848View attachment 42849

Only took about 15 minutes too!

 
Last edited by a moderator:
I used to use the caustic soda for bike parts that I want to change colour on....

I found that leaving it in a bit too long created a satin black finish that was a bugger to  remove , but replicated a DLC sort of finish.

Worth trying on those tired looking parts , though it would I'm sure eventually cause damage to the metal , so its a practice makes perfect with the timing situation (my disclaimer!) ?

 
Last edited by a moderator:
I used to use the caustic soda for bike parts that I want to change colour on....

I found that leaving it in a bit too long created a satin black finish that was a bugger to  remove , but replicated a DLC sort of finish.

Worth trying on those tired looking parts , though it would I'm sure eventually cause damage to the metal , so its a practice makes perfect with the timing situation (my disclaimer!) ?


Totally. Research is key.

I've heard stories of people making the solution very strong and in the space of an hour the aluminium part has literally dissolved... Nothing but particles of metal in water, hahahaha.

I'm not that stupid.

Start weak and get stronger if it's taking too long and NEVER leave it unattended. Easy as pie and no damage.

PS. The satin black finish you refer to is called smut. Easily removed but at that point it has started attacking the metal and not just the very thin oxidised layer. Basically burnt metal.

 
Last edited by a moderator:
Cheers dude! I do try!

Not bad for a first pistol... And first Airsoft weapon...

Will be much better when it's fully finished. You can expect pictures! lol
First pistol!!! Bloody hell flash as fuck mate and your first RIF please tell me you're not another one of those maniacs that run all over the place scaring the shit out of us older folk ?

 
please tell me you're not another one of those maniacs that run all over the place scaring the shit out of us older folk ?


Depends on the situation... but yes... im aggressive pistol only ?

edit: but im not exactly a spring chicken myself, lol

 
Last edited by a moderator:
Back
Top